機(jī)壓
Pressing
MS-80 |
機(jī)壓
Pressing
MS-85 |
澆注
Slip Casting
CM-80 |
Al2O3(%) |
≥80 |
≥85 |
≥80 |
SiO2(%) |
≤18 |
≤13 |
≤18 |
Fe2O3(%)
|
≤0.5 |
≤0.5 |
≤0.5 |
顯氣孔率(%)
Apparent Porosity |
≤17 |
≤17 |
≤23 |
容重(g/cm3)
Bulk Density |
≥2.75 |
≥2.85 |
≥2.50 |
荷重軟化始點(diǎn)T0.6(℃)
Refractoriness under load |
≥1680 |
≥1700 |
≥1650 |
冷壓強(qiáng)度(MPa)
Cold Crushing strength |
≥100 |
≥100 |
≥90 |
※所列技術(shù)指標(biāo)均為同牌號產(chǎn)品標(biāo)準(zhǔn)磚的檢測數(shù)據(jù)
All chemical-physical data are obtained based on the corresponding refractory bricks of standard size.
用途:
玻璃熔窯上部結(jié)構(gòu)、通道、成型部件。
Applications:
Superstructures, forehearths, forming parts.
|